| Sign In | Join Free | My futurenowinc.com |
|
Material : X1CrNiMoN25-22-2
Steel number : 1.4466
Type : stainless steel pipes
standard : en10216-5
| Grade : | X1CrNiMoN25-22-2 | ||||||||
| Number: | 1.4466 | ||||||||
| Classification: | Austenitic stainless steel - special grade | ||||||||
| Density: | 8 g/cm ³ | ||||||||
| Standard: |
|
| Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast. |
| C | Si | Mn | Ni | P | S | Cr | Mo | N |
| max 0.02 | max 0.7 | max 2 | 21 - 23 | max 0.025 | max 0.01 | 24 - 26 | 2 - 2.5 | 0.1 - 0.16 |
| Rm - Tensile strength (MPa) (+A) | 540-740 |
| Rm - Tensile strength (MPa) (+AT) | 540-740 |
| Rp0.2 0.2% proof strength (MPa) (+A) | 250 |
| Rp0.2 0.2% proof strength (MPa) (+AT) | 260 |
| KV - Impact energy (J) transverse, (+A) | +20° 60 | -196° 60 |
| KV - Impact energy (J) longitud., (+A) | +20° 100 |
| A - Min. elongation at fracture (%) (+A) | 35-40 |
| A - Min. elongation at fracture (%) longitud., (+AT) | 40 |
| A - Min. elongation at fracture (%) transverse, (+AT) | 30 |
| Brinell hardness (HB): (+A) | 240 |
| Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes Steel shal not be applied at a metal temperature lower than -270 ° C |
| EU EN | USA - | France AFNOR | ||
| X1CrNiMoN25-22-2 |
|
|
|
|
X1CrNiMoN25-22-2 Heat Resistant Stainless Steel Pipe EN 10216-5 1.4466 Steel Pipe Images |